Process for preparing a hydrotreating catalyst
US9993809B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Nov 4, 2014 |
| Grant date | Jun 12, 2018 |
| Priority date | — |
| Expiry date | Nov 4, 2034 |
Classification
- Technology area (CPC B)Performing Operations; Transporting
- CPC primaryB01J2523/00
- WIPO fieldChemical engineering
- WIPO sectorChemistry
Abstract
Process for preparing a hydrotreating catalyst comprising of from 5 wt % to 50 wt % of molybdenum, of from 0.5 wt % to 20 wt % of cobalt, and of from 0 to 5 wt % of phosphorus, all based on total dry weight of catalyst, which process comprises (a) treating a nickel containing carrier with molybdenum, cobalt and of from 1 to 60% wt of gluconic acid, based on weight of carrier, and optionally phosphorus, (b) optionally drying the treated carrier at a temperature of from 40 to 200° C., and (c) calcining the treated and optionally dried carrier at a temperature of from 200 to 650° C. to obtain the calcined treated carrier.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.