Cemented carbide body with increased wear resistance
USRE41646E1 · kind E1 · reissue
Assignee
Inventors
Key dates
| Filing date | Jul 8, 1997 |
| Grant date | Sep 7, 2010 |
| Priority date | — |
| Expiry date | Jul 8, 2017 |
Classification
- Technology area (CPC —)General
Abstract
As there is disclosed a cemented carbide body comprising WC with an average grain size of <10 μm in a binder phase. In the cemented carbide body the WC grains can be classified in at least two groups in which a group of smaller grains has a maximum grain size amax and a group of larger grains has a minimum grain size bmin and each group contains at least 10 % of the total amount of WC grains. According to the invention bmin−amax>0.5 μm and the difference in grain size within each group is >1 μm.