Most-cited inventions
| Patent | Title | Area | Cited by | Status |
|---|---|---|---|---|
| US4749594A | Method for coating surfaces with hard substances | Chemistry; Metallurgy | 27 | Expired |
| US4341556A | Material for electrical contacts | Chemistry; Metallurgy | 9 | Expired |
| US4344794A | Solder alloy for the direct soldering of oxide containing silver catalyst on catalyst carrier | Performing Operations; Transporting | 6 | Expired |
| US7432790B2 | Superconductor assembly | Electricity | 4 | Expired |
| US8173901B2 | Multifilament superconductor, as well as method for its production | Emerging Cross-Sectional Technologies | 1 | Active |
| US9251931B2 | NbTi superconductor with peripherally distributed Al block for weight reduction | Emerging Cross-Sectional Technologies | 0 | Active |
| US9147507B2 | NbTi superconductor with reduced weight | Electricity | 0 | Active |
| US8318639B2 | Superconducting composite, preliminary product of superconducting composite and method for producing same | Emerging Cross-Sectional Technologies | 0 | Active |
| US9177699B2 | Method for producing a superconducting wire, in particular using lead-free solder | Emerging Cross-Sectional Technologies | 0 | Active |
Source: USPTO / EPO open patent data. Inventor disambiguation is heuristic; counts are objective bibliographic measures.