Patent · US Active

Spray-formed high-speed steel

US10233519B2 · kind B2 · utility

0Cited by
30References
20Claims
0Family size

Assignees

Inventors

Key dates

Filing dateSep 30, 2015
Grant dateMar 19, 2019
Priority date
Expiry dateApr 5, 2036

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C38/26
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A spray-formed high-speed steel includes chemical components by mass percent of: C: 0.85-1.65%, Si: 0.1-1.2%, Cr: 3.5-8.0%, W: 4.0-6.5%, Mo: 4.5-7.0%, V: 1.0-4.0%, Co: 1.0-8.0%, Mn: 0.2-0.8%, and Nb: 0.2-3.5%, with balance of iron and impurities.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.