Patent · US Active

Solder bonding method and solder joint

US11097379B2 · kind B2 · utility

0Cited by
4References
7Claims
0Family size

Assignee

Inventors

Key dates

Filing dateFeb 15, 2019
Grant dateAug 24, 2021
Priority date
Expiry dateNov 14, 2039

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P70/50
  • WIPO fieldMachine tools
  • WIPO sectorMechanical engineering

Abstract

A solder bonding method that bonds, using a solder joint, an electrode of a circuit board to an electrode of an electronic component includes: depositing, on the electrode of the circuit board, an Sn—Bi-based solder alloy with a lower melting point than a solder alloy deposited on the electrode of the electronic component; mounting the electronic component on the circuit board such that the Sn—Bi-based solder alloy contacts the solder alloy on the electrode of the electronic component; heating the circuit board to a peak temperature of heating of 150° C. to 180° C.; holding the peak temperature of heating at a holding time of greater than 60 seconds and less than or equal to 150 seconds; and cooling, after the heating and to form the solder joint, the circuit board at a cooling rate greater than or equal to 3° C./sec.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.