A method of manufacturing a copper nano-ink includes: a step of preparing a copper nanoparticle aqueous dispersion liquid including copper nanoparticles and anions; and a step of storing the copper nanoparticle aqueous dispersion liquid at 5° C. or less after the step of preparing, wherein in the step of storing, a copper ion concentration of the copper nanoparticle aqueous dispersion liquid is controlled to be greater than or equal to 0.1 g/L and less than or equal to 1.0 g/L and an anion concentration is controlled to be greater than or equal to 0.5 g/L and less than or equal to 8.0 g/L.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.