Patent · US Expired

Process for preparing a calcium silicate shaped product

US4490320A · kind A · utility

4Cited by
1References
15Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 28, 1982
Grant dateDec 25, 1984
Priority date
Expiry dateDec 28, 2002

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC04B28/18
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A process for preparing a calcium silicate shaped product comprises heat-reacting a calcareous source and a siliceous source dispersed in water to obtain an aqueous slurry containing a calcium silicate hydrate having a molar ratio of CaO/SiO.sub.2 being more than 1, adding a siliceous source to the aqueous slurry to bring the molar ratio of CaO/SiO.sub.2 to a level of from 0.85 to 1, and pressfilter-molding the aqueous slurry thereby obtained, followed by steam-curing and drying.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.