Tube having strain-hardened inside coating

US4641450A · kind A · utility

22Cited by
6References
5Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 18, 1985
Grant dateFeb 10, 1987
Priority date
Expiry dateApr 18, 2005

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/13
  • WIPO fieldSurface technology, coating
  • WIPO sectorChemistry

Abstract

To manufacture tubes having a wear-resistant inside coating, such as gun barrels, hard material layers are deposited on the barrel and the layers are strain-hardened in their surface area by at least the ratio of the area by which the surface area is reduced by compression divided by the surface area of 0.001 (.DELTA.F/F=1.10.sup.-3) or reducing the area of the layer by 0.1%.