Patent · US Expired

Thermoplastic olefin elastomer

US4713419A · kind A · utility

11Cited by
9References
4Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 30, 1986
Grant dateDec 15, 1987
Priority date
Expiry dateApr 30, 2006

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08L2207/04
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

There is provided a thermoplastic olefin elastomer of polyblend composed of 30 to 70 wt % of ethylene-propylene-diene terpolymer (EPDM), 10 to 30 wt % of ethylene-vinyl acetate copolymer (EVA), and 20 to 50 wt % of polypropylene (PP). The EPDM is specified by the Mooney viscosity, propylene content, and third component. The EVA is specified by the VA content and number-average molecular weight. The PP is specified by the number-average molecular weight. This elastomer is suitable for use as a raw material for automotive exterior trim such as side molding, bumper, and mud guard which are produced by injection molding. The elastomer also affords molded items having a good matte-finished appearance. The polyblend obviates the process for partial crosslinking which was necessary for the preparation of conventional elastomer for injection molding.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.