Method of manufacture of thermoplastic elastomer compounds
US4801651A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Nov 2, 1987 |
| Grant date | Jan 31, 1989 |
| Priority date | — |
| Expiry date | Nov 2, 2007 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08L2666/04
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
(A) polypropylene (10-90 weight part), (B) halogenated butyl rubber (90-10 weight part, (A)+(B)=100 weight part), (C) olefinic rubber (10-120 weight part) and (D) mineral oil softening agent (5-120 weight part) are heated in the presence of (E) metal oxide and/or metal chloride. To 100 weight part of the resulting composition are added, (F) polyolefin (100-600 weight part) and (G) vulcanizable olefinic rubber (50-500 weight part) and the components are mixed and heated in the presence of (H) organic peroxide. The resulting thermoplastic elastomer composition has good paintability, moldability, compatibility, low temperature impact strength, and especially high stiffness at elevated temperature.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.