Patent · US Expired

Method of producing fluorapatite

US4855118A · kind A · utility

13Cited by
2References
3Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 12, 1988
Grant dateAug 8, 1989
Priority date
Expiry dateApr 12, 2008

Classification

  • Technology area (CPC G)Physics
  • CPC primaryG01N27/121
  • WIPO fieldMeasurement
  • WIPO sectorInstruments

Abstract

A method of producing fluorapatite wherein predetermined amounts of calcium monohydrogen phosphate, calcium carbonate, and calcium fluoride are weighed, subjected to a mechanochemical action, and caused to react with one another in water. With this method, a fluorapatite having a uniform composition can be obtained without the accompaniment of by-products. A moisture sensitive resistor of the present invention can be obtained by sintering the fluorapatite produced in accordance with this method. This moisture sensitive resistor has a sufficiently low resistance corresponding to a humidity, and has substantially no hysteresis.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.