Abstract
This invention relates to alkyl and alkanol sulfonic acid plating baths and to methods for plating tin and tin-lead alloys. It also relates to low foaming wetting systems based on low to moderate foaming surfactants and soluble, non-silicon containing defoamers, and to low volatility brightener systems.