Method of forming metal or metal silicide film

US5175017A · kind A · utility

32Cited by
1References
57Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJan 28, 1991
Grant dateDec 29, 1992
Priority date
Expiry dateJan 28, 2011

Classification

  • Technology area (CPC H)Electricity
  • CPC primaryH01L21/76877
  • WIPO fieldSemiconductors
  • WIPO sectorElectrical engineering

Abstract

In forming a metal or metal silicide film by CVD, a fluorosilane is used as a reaction gas, or a fluoro-silane is added to a source gas. Examples of the metal halide used in the present invention include fluorides and chlorides of tungsten, molybdenum, titanium, tantalum and niobium. Among them, fluorides of tungsten and molybdenum are more desirable particularly from the viewpoint of the availability of the deposited metal or metal silicide. It is preferred that the source gases, i.e. silane series gas and metal halide, be diluted with a carrier gas such as nitrogen, hydrogen, helium or argon, and this is also true of the fluoro-silane. The total pressure is preferably 0.01 to 10 Torr. The reaction temperature is desirably 200.degree. to 800.degree. C., more desirably 300.degree. to 500.degree. C. Plasma CVD instead of thermal CVD may be employed for the purpose of lowering the reaction temperature.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.