Method of manufacturing semiconductor device and semiconductor device
US6509648B1 · kind B1 · utility
Assignee
Inventors
Key dates
| Filing date | Oct 19, 2000 |
| Grant date | Jan 21, 2003 |
| Priority date | — |
| Expiry date | Feb 8, 2021 |
Classification
- Technology area (CPC H)Electricity
- CPC primaryH01L21/76819
- WIPO fieldSemiconductors
- WIPO sectorElectrical engineering
Abstract
A method of manufacturing a semiconductor device is obtained which is capable of evading generation of a short circuit between wirings in an upper wiring layer even if a part of an upper surface of an FSG film is exposed by variations in a production step. After a USG film (4) is deposited to a thickness of 1 Hm over an entire surface of an FSG film (3), the USG film (4) is polished and removed by a thickness of 900 nm from an upper surface thereof by the CMP method. At this time, part of an upper surface of the FSG film (3) is exposed by variations in a production step. Next, the surface of the interlayer dielectric film (50) is cleaned with a cleaning liquid whose etching rate to the FSG film (3) and etching rate to the USG film (5) are substantially the same. Such a cleaning liquid may be, for example, an ammonia hydrogen peroxide mixture of NH4OH:H2O2:H2O=1:1:20. The structure shown in FIG. 5 is dipped in the above-mentioned ammonia hydrogen peroxide mixture for 60 seconds to clean the surface of the interlayer dielectric film (50).
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.