Patent · US Expired

Method of manufacturing a contact interconnection layer containing a metal and nitrogen by atomic layer deposition for deep sub-micron semiconductor technology

US7235482B2 · kind B2 · utility

509Cited by
20References
23Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 8, 2003
Grant dateJun 26, 2007
Priority date
Expiry dateFeb 7, 2024

Classification

  • Technology area (CPC H)Electricity
  • CPC primaryH01L2924/0002
  • WIPO fieldSemiconductors
  • WIPO sectorElectrical engineering

Abstract

An atomic layer deposition method is used to deposit a TiN or TiSiN film having a thickness of about 50 nm or less on a substrat. A titanium precursor which is tetrakis(dimethylamido)titanium (TDMAT), tetrakis(diethylamido)titanium (TDEAT), or Ti{OCH(CH3)2}4 avoids halide contamination from a titanium halide precursor and is safer to handle than a titanium nitrate. After a monolayer of the titanium precursor is deposited on a substrate, a nitrogen containing reactant is introduced to form a TiN monolayer which is followed by a second purge. For TiSiN, a silicon source gas is fed into the process chamber after the TiN monolayer formation. The process is repeated several times to produce a composite layer comprised of a plurality of monolayers that fills a contact hole. The ALD method is cost effective and affords an interconnect with lower impurity levels and better step coverage than conventional PECVD or CVD processes.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.