Double anneal with improved reliability for dual contact etch stop liner scheme
US8148221B2 · kind B2 · utility
Assignees
Inventors
Key dates
| Filing date | Oct 19, 2009 |
| Grant date | Apr 3, 2012 |
| Priority date | — |
| Expiry date | Oct 20, 2029 |
Classification
- Technology area (CPC H)Electricity
- CPC primaryH10D84/0184
- WIPO fieldSemiconductors
- WIPO sectorElectrical engineering
Abstract
A method for forming a device with both PFET and NFET transistors using a PFET compressive etch stop liner and a NFET tensile etch stop liner and two anneals in a deuterium containing atmosphere. The method comprises: providing a NFET transistor in a NFET region and a PFET transistor in a PFET region. We form a NFET tensile contact etch-stop liner over the NFET region. Then we perform a first deuterium anneal. We form a PFET compressive etch stop liner over the PFET region. We form a (ILD) dielectric layer with contact openings over the substrate. We perform a second deuterium anneal. The temperature of the second deuterium anneal is less than the temperature of the first deuterium anneal.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.