Method to generate high LSG low-emissivity coating with same color after heat treatment
US9790127B2 · kind B2 · utility
1Cited by
13References
11Claims
0Family size
Assignees
Inventors
Key dates
| Filing date | Mar 14, 2013 |
| Grant date | Oct 17, 2017 |
| Priority date | — |
| Expiry date | Mar 14, 2033 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/265
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
Low emissivity panels can include a separation layer of Zn2SnOx between multiple infrared reflective stacks. The low emissivity panels can also include NiNbTiOx as barrier layer. The low emissivity panels have high light to solar gain, color neutral, together with similar observable color before and after a heat treatment process.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.