Abstract
A method for fabricating a semiconductor device includes depositing a sacrificial liner in self-aligned contact openings in first and second regions. The openings are filled with a sacrificial material. The second region is blocked with a first mask to remove the sacrificial material from the first region. The first mask is removed from the second region, and the sacrificial liner is removed from the first region. A first liner is formed in the openings of the first region, and first contacts are formed in the first region on the first liner. The first region is blocked with a second mask to remove the sacrificial material from the second region. The second mask is removed from the first region, and the sacrificial liner is removed from the second region. A second liner is formed in the openings of the second region, and second contacts are formed in the second region.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.