Treatment of silicon prior to nickel silicide formation

US7132365B2 · kind B2 · utility

1Cited by
6References
10Claims
0Family size

Assignee

Inventors

Key dates

Filing dateAug 10, 2004
Grant dateNov 7, 2006
Priority date
Expiry dateAug 10, 2024

Classification

  • Technology area (CPC H)Electricity
  • CPC primaryH01L21/76829
  • WIPO fieldSemiconductors
  • WIPO sectorElectrical engineering

Abstract

A method of preparing a die comprises treating exposed silicon to form an oxide prior to silicide formation; and depositing metal on the oxide. The metal may comprise titanium, cobalt, nickel, platinum, palladium, tungsten, molybdenum, or combinations thereof on the oxide. The oxide may be less than or equal to about 15 angstroms thick. In various embodiments, treating exposed silicon to form an oxide comprises forming a non-thermal oxide. Treating exposed silicon to form an oxide may also comprise treating the exposed silicon with an oxidizing plasma; alternatively, treating exposed silicon to form an oxide may comprise forming a chemical oxide. In certain other embodiments, treating exposed silicon to form an oxide comprises treating exposed silicon with a solution comprising ammonium hydroxide, hydrogen peroxide, and water; hydrochloric acid, hydrogen peroxide, and water; hydrogen peroxide; ozone; ozonated deionized water; or combinations thereof.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.