Patent · US Active

Semiconductor device and method of manufacturing the same

US8563415B2 · kind B2 · utility

0Cited by
2References
11Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 24, 2010
Grant dateOct 22, 2013
Priority date
Expiry dateJan 28, 2031

Classification

  • Technology area (CPC H)Electricity
  • CPC primaryH10D64/691
  • WIPO fieldSemiconductors
  • WIPO sectorElectrical engineering

Abstract

The present invention relates to a method of manufacturing a semiconductor device. After depositing the metal gate electrode material, a layer of oxygen molecule catalyzing layer having a catalyzing function to the oxygen molecules is deposited, and afterwards, a low-temperature PMA annealing process is used to decompose the oxygen molecules in the annealing atmosphere into more active oxygen atoms. These oxygen atoms are diffused into the high-k gate dielectric film through the metal gate to supplement the oxygen vacancies in the high-k film, in order to alleviate oxygen vacancies in the high-k film and improve the quality of the high-k film. According to the present invention, the oxygen vacancies and defects of high-k gate dielectric film will be alleviated, and further, growth of SiOx interface layer having a low dielectric constant caused by the traditional PDA high temperature process may be prevented. Thereby, the EOT of the entire gate dielectric layer may be effectively controlled, and the MOS device may be continuously scaled. Meanwhile, the present invention further provides a semiconductor device obtained according to the above-mentioned method.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.