Method of manufacturing a CPP structure with enhanced GMR ratio
US8484830B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Apr 4, 2011 |
| Grant date | Jul 16, 2013 |
| Priority date | — |
| Expiry date | Jul 31, 2031 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/115
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
A CPP-GMR spin valve having a CoFe/NiFe composite free layer is disclosed in which Fe content of the CoFe layer ranges from 20 to 70 atomic % and Ni content in the NiFe layer varies, from 85 to 100 atomic % to maintain low Hc and λs values. A small positive magnetostriction value in a Co75Fe25 layer is used to offset a negative magnetostriction value in a Ni90Fe10layer. The CoFe layer is deposited on a sensor stack in which a seed layer, AFM layer, pinned layer, and non-magnetic spacer layer are sequentially formed on a substrate. After a NiFe layer and capping layer are sequentially deposited on the CoFe layer, the sensor stack is patterned to give a sensor element with top and bottom surfaces and a sidewall connecting the top and bottom surfaces. Thereafter, a dielectric layer is formed adjacent to the sidewalls.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.