A method of high aspect ratio contact etching a substantially vertical contact hole in an oxide layer using a hard photoresist mask is described. The oxide layer is deposited on an underlying substrate. A plasma etching gas is formed from a carbon source gas. Dopants are mixed into the gas. The doped plasma etching gas etches a substantially vertical contact hole through the oxide layer by doping carbon chain polymers formed along the sidewalls of the contact holes during the etching process into a conductive state. The conductive state of the carbon chain polymers reduces the charge buildup along sidewalls to prevent twisting of the contact holes by bleeding off the charge and ensuring proper alignment with active area landing regions. The etching stops at the underlying substrate.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.