Patent · US Active

Deposition of boron and carbon containing materials

US9576790B2 · kind B2 · utility

6Cited by
15References
26Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 14, 2015
Grant dateFeb 21, 2017
Priority date
Expiry dateApr 14, 2035

Classification

  • Technology area (CPC H)Electricity
  • CPC primaryH01L21/31111
  • WIPO fieldSemiconductors
  • WIPO sectorElectrical engineering

Abstract

Methods of depositing boron and carbon containing films are provided. In some embodiments, methods of depositing B, C films with desirable properties, such as conformality and etch rate, are provided. One or more boron and/or carbon containing precursors can be decomposed on a substrate at a temperature of less than about 400° C. One or more of the boron and carbon containing films can have a thickness of less than about 30 angstroms. Methods of doping a semiconductor substrate are provided. Doping a semiconductor substrate can include depositing a boron and carbon film over the semiconductor substrate by exposing the substrate to a vapor phase boron precursor at a process temperature of about 300° C. to about 450° C., where the boron precursor includes boron, carbon and hydrogen, and annealing the boron and carbon film at a temperature of about 800° C. to about 1200° C.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.